Before and after Extreme Pressure Additive
Gary Rodak phone 734-904-4060 Gary.Rodak_at_Machin
ingEfficiencies.com
  • Photo on left (before additive, original wear
    patterns) depicts a fair amount of diffusion
    wear.
  • Once that was cured with an EP additive, the next
    form of wear experienced is chipping and/or
    fracture wear.
  • Photo on right indicates that an increase in
    surface feet per minute may reduce this wear
    pattern.
  • Wear like this may be related to a lack of tool
    holder rigidity or re-circulated fines.
  • Both conditions are with identical (proper)
    coolant flow practices, equal number of parts and
    machine data setup.
  • Recommendation Increase Surface Feet per Minute
    by 10. Maintain the same feed rate per
    revolution.