Title: 1' INTRODUCTION GENERAL PRINCIPLES AND BASIC CONCEPTS
1- 1. INTRODUCTION GENERAL PRINCIPLES AND BASIC
CONCEPTS - Composites in the real world Classification of
composites scale effects the role of
interfacial area and adhesion three simple
models for a-priori materials selection the role
of defects Stress and strain thermodynamics of
deformation and Hookes law anisotropy and
elastic constants micromechanics models for
elastic constants Lectures 1-2 - 2. MATERIALS FOR COMPOSITES FIBERS, MATRICES
- Types and physical properties of fibers
flexibility and compressive behavior stochastic
variability of strength types and physical
properties of matrices combining the phases
residual thermal stresses Lectures 3-5 - 3. THE PRINCIPLES OF FIBER REINFORCEMENT
- Stress transfer The model of Cox The model of
Kelly Tyson Other model Lectures 6-7 - 4. INTERFACES IN COMPOSITES
- Basic issues, wetting and contact angles,
interfacial adhesion, the fragmentation - phenomenon, microRaman spectroscopy,
transcrystalline interfaces, Lectures 8-9 - 5. FRACTURE PHYSICS OF COMPOSITES
- Griffith theory of fracture, current models for
idealized composites, stress concentration,
simple mechanics of materials, micromechanics of
composite strength, composite toughness Lectures
10-11 - 6. DESIGN EXAMPLE
- A composite flywheel Lecture 12
2Types and physical properties of matrices
3Thermosets
- Heavily crosslinked polymers consisting of a
rigid 3d molecular network - Upon the application of heat, they degrade rather
than melt - Initial uncured state low viscosity
- Curing ( polymerization) involves chain
extension, branching, crosslinking. This leads to
rigidity, strength, solvent resistance, good
thermal/oxidative stability - Sensitivity to moisture use temperature limit
200 C - Polyesters, epoxies
4Preparation of epoxy resin
STEP 1
GROUP
epoxy
glycidyl
REACTANTS
epichlorohydrin
Bisphenol A
epoxy
5STEP 2
Reaction of an epoxide group with a diethylene
triamine (DETA) molecule ( the curing agent, or
hardener)
6STEP 3
Formation of crosslinks
7TYPES OF HARDENERS Anhydrides provide good
electrical insulating properties, thermal
resistance, environmental stability Aromatic
amines provide higher thermal resistance but
require higher cure T Aliphatic amines lead to
fast cure, suited to room T curing of epoxy ROLE
OF HARDENERS Reduce curing time, achieve
desirable properties
8EXAMPLES OF EPOXIES
DGEBA
NOVALAC (Dow DEN 438)
9SHELL EPON 1031
Ciba Geigy MY-720
10- Curing can be achieved at room temperature but
is usually performed at higher temperatures (for
shorter times). A postcure at relatively high
temperature is usually added to avoid further
(unwanted) property change during service. - Shrinkage during cure, thermal contraction upon
cooling after cure lead to built-in residual
stresses in composites. - Thermosets are usually isotropic, homogeneous
solids. - Thermosets loose their stiffness at the Heat
Distorsion Temperature (HDT) upper structural
limit. - High-temperature thermosets include polyimides
(PIs), bismaleimides (BMI), etc. due to
aromatic structures
11Types and physical properties of matrices
Not treated here, limited use in composites in
general (tires)
12THERMOPLASTICS
- Advantages easier to use, faster to prepare,
cheaper, longer shelf life, tougher, higher
temperature use - Not crosslinked. Origin of their
strength/stiffness is the inherent properties of
monomer unit, and the high molecular weight. - Amorphous thermoplastics high concentration of
molecular entanglements (act like crosslinks).
Heating leads to disentanglement (rigid to
viscous) - Crystalline thermoplastics high degree of
molecular order, alignment. Heating leads to
melting (sharp melting point) - Examples Polypropylene (semi-cryst), nylon
(semi-cryst), polycarbonate (amorphous) - Creep under load
- Phenomenon of transcrystallinity
13TRANSCRYSTALLINITY
HM graphite fiber in PP. The fiber acts as a
nucleating agent, heterogeneous nucleation arises.
14(No Transcript)
15(No Transcript)
16RESIDUAL THERMAL STRESSES
- First, some experimental observations
- Metal-matrix composites Large difference
between TEC (a) of fiber and matrix, leading to
interface or matrix cracking. And DT is very
large, inducing fracture. Example SiC/Ti - Thermoplastic polymer matrix composites Same as
above, very high Da, DT. Moreover, fibers that
are weak in compression break following sample
preparation (spontaneous fragmentation). Example
HM graphite/polypropylene
17(No Transcript)
18Compressive breaks in HM graphite fiber embedded
in isotactic PP
19Compressive shrinkage arises in thermoset
matrices as well
20These compressive phenomena are attributed to
residual thermal stresses during specimen
preparation.
- QUESTIONS
- What is the magnitude of these stresses?
- Under which conditions and for which materials do
such stresses become a critical problem for a
structure?
Theoretical models schemes exist for (1)
one-dimensional models, and (2) isotropic
homogeneous shrink-fit concentric cylinders
with perfect interface.
21One-dimensional model
- Main hypothesis only z (longitudinal) (residual)
stress components exist in the fibers and matrix - Secondary hypothesis E and a are not
temperature-dependent
Eq. 1
where a coefficient of thermal expansion E
Youngs modulus T temperature (Tref
stress-free reference temperature) f volume
fraction
223D models
- Composite (concentric) cylinders model
- Reference papers
- J.A. Nairn, Polymer Composites 6(2) (1985),
123-130 - H.D. Wagner, Physical Review B, 53 (9) (1 March
1996-I), 5055-5058. - H.D. Wagner, J.A. Nairn, Composites Science and
Technology, 57 (9-10) (1997), 1289-1302.
History (1) 1934 fabrication of guns
(Poritski) (2) 1962 Glass/epoxy composites
(Haslett McGarry) (3) 3 cylinder solution,
anisotropic fiber, isotropic interlayer and
matrix (Nairn).
Schematic overview of the (simple version of the)
model for 2 cylinders only There are 3 steps
23One hollow cylinder Classical solution exists
for a linear elastic, isotropic cylinder
subjected to internal and external pressure
(P)i designates internal or in, o
designates external or out
HOLE
CYLINDER
For the radial, hoop and longitudinal stresses in
the cylinder. The parameter x is a constant.
242. Next, we consider 2 concentric cylinders
internal cylinder is a solid fiber external
cylinder is hollow matrix.
Both cylinders are transversally isotropic rather
than isotropic ! In cylindrical coordinates
2 indept TECs
4 indept elastic constants
n Poisson ratio, E Youngs modulus, DT T -
Tref
25It can be shown stresses in transversally
isotropic cylinders are the same as for the
isotropic case (which were just presented).
For the internal cylinder (the fiber), internal
pressure Pi 0, internal radius Ri 0. Thus,
the equations (of step 1 above) become for the
fiber
where Afiber and Cfiber are constants.
For the external cylinder (the matrix), external
pressure Po 0. Thus, the equations (of step 1
above) become for the matrix
where Amatrix , Bmatrix, Cmatrix are constants.
26- Therefore, five unknows Af, Cf, Am, Bm, Cm.
- Radial stress boundary conditions
_at_ r R2
_at_ r R1
- Force balance in longitudinal direction
This leads to
So there are only 2 unknowns left
27To determine the 2 unknowns (AM and CM), combine
stress-strain relations with interfacial no-slip
conditions
Both _at_ r R1 (and u displacement)
But since ur r eqq, the above is equivalent to
_at_ r R1
These no-slip conditions combined with
stress-strain relations yield 2 simultaneous eqs
with 2 unknowns
28With
and
(These reduce to Nairns elements (1985) if the
matrix is isotropic)
29Solving the system of 2 equations with 2 unknowns
leads to
By inserting these into the earlier expressions
for BM, AF, CF, the residual thermal stresses in
both the fiber and the matrix may be determined.
30- Finally, we must consider 3 concentric cylinders
internal cylinder is a solid fiber middle
cylinder is hollow interphase external
cylinder is hollow matrix. The cylinders are
transversally isotropic. The solution is similar
as for the 2 cylinder case, but more complex (see
referenced papers).
- Illustrative examples using HM graphite/polypropyl
ene composites - Key questions
- What is the effect of volume fraction on residual
stresses? - Can we predict the amount of fiber compressive
breaks generated by residual stresses as a
function of DT?
31(No Transcript)
32MICROCOMPOSITE (very small volume
fraction) Large compressive stresses are induced
in the fiber, as the materials cools.
33MACROCOMPOSITE (large volume fraction) Small
compressive stresses are induced in the fiber, as
the materials cools.
34Comparison between volume fractions on a single
plot
35Microcomposite
36Macrocomposite
37SUMMARY IN TABULAR FORM, FOR DIFFERENT COMPOSITES
CONCLUSIONS Criticality in micromechanical
testing mostly
38 predictive tool for the effect of large
compressive stresses in fibers (of the order of
100,000 Atmospheres!)
Can we also predict the number of fiber breaks as
a function of DT?
Assumption The compressive fiber strength
follows a Weibull distribution. Then the ratio of
average compressive strengths of two fiber
populations with lengths L1 and L2 is
To predict the strength for any other length, we
need to know one pair of values (Li, ltsgtLi), and
the shape parameter b.
39ltsgtLi may be viewed as the average compressive
strength of a fiber fragment of length Li. The
average fragment length at stress level ltsgtLi is
equal to L0/Ni where L0 is the original
(unbroken) fiber length and Ni is the average
number of breaks. Therefore, for two populations
with fragment lengths L1 and L2, one has
In particular, when L1 L0, we have N1 1 and
the average number of fiber breaks up to ltsgtLi is
()
40- For a given value of the undercooling DT, one
calculates the residual stress level ltsgtLi in the
fiber using the models developed earlier. From
this, the number of breaks can be derived via the
expression () above. - EXAMPLE Literature data for HM graphite/PP
suggests a compressive strength of 1.08 GPa for
a 10 mm gauge length fiber. Using () we find
This leads to the following predictive plot for 2
values of b
41(No Transcript)
42How do we know which curve is correct? By
comparison with experiments in which the number
of breaks per unit length is found to vary
between 5 and 8.5 breaks per mm under DT -130
C, we see that the curve for b 2 gives a
fairly good fit. Alternatively, the fiber
volume fraction may be varied and the number of
spontaneous breaks counted per unit length. This
gives the following plot
43As predicted, there are many more breaks at low
fiber content than at high fiber content.
Calculated values of N provide the following plot
44Again, the best-fit value for b is in the range
1.5 to 2.