Title: Measurements on SPS sample in C-magnet
1Progress on coatings, SPS samples and e-cloud
measurements
Measurements on SPS sample in C-magnet SPS MD
run 12.8 Coating system prototype for SPS
magnets
TS-MME, AT-VAC, AB/OP-RF-BI-ABP
2Chamber for sample insertion in SPS C-magnet
J.Axensalva
Sample location
3Sample SPS-SEY, 316 LN, after scrubbing run 8/7
and first MD
edge, holder
-Conditioned region well visible in the central
part, with yield down to 1.54 (dose 0.01-0.02
Clb/cm) -Clean non-conditioned stainless steel
has SEY 2.4-2.5 -During transfer p1x10-4 mbar
for 1h (pumped down to 5x10-5mbar for transfer)
4XPS on the same sample
Carbon concentration
-More C on conditioned zone -Different C1s
binding energy (C is more graphitic?....)
285eV
285.4eV
285.6eV
285.6eV
5Results 2nd MD run (12.8)
Magnets on
6Results 2nd MD run (12.8)
d1.25 after 15d in air but second measurement
on same sample
magnet on
Effect of bad vacuum?
7Design of cathode system for coating test in an
SPS magnet (building 181)